Laser-induced breakdown spectroscopy (LIBS) is used to analyze chemically etched polytetrafluoroethylene (PTFE). The elements O, F, H, and Na are determined qualitatively in the depth dimension. It is shown that O, H, and Na signals are greatest at the surface and decrease as the laser burrows through the etched layer into the bulk. In contrast, the fluorine signal is a minimum at the surface and increases with depth. The average ablation rate for PTFE under the experimental conditions is found to be 1.9 μm per pulse. Using this value, the depth of the etched layer is determined to be 8 μm. A calibration curve produced by analysis of different polymers gives mole fractions of O, F, and H at the surface of the etched PTFE of 0.2, 0.3, and 0.1, respectively.
PDF Article
More Like This
Cited By
You do not have subscription access to this journal. Cited by links are available to subscribers only. You may subscribe either as an Optica member, or as an authorized user of your institution.
Contact your librarian or system administrator
or
Login to access Optica Member Subscription